z-logo
open-access-imgOpen Access
Effects of doping concentration and sintering temperature on luminescence of CaWO4:Eu3+ phosphor
Author(s) -
Yang Gao,
Luuml; Qiang,
Yang Wang,
Zhan-Bo Liu
Publication year - 2012
Publication title -
wuli xuebao
Language(s) - English
Resource type - Journals
SCImago Journal Rank - 0.199
H-Index - 47
ISSN - 1000-3290
DOI - 10.7498/aps.61.077802
Subject(s) - phosphor , doping , materials science , sintering , ion , luminescence , analytical chemistry (journal) , microemulsion , chemical engineering , mineralogy , optoelectronics , environmental chemistry , composite material , chemistry , pulmonary surfactant , organic chemistry , engineering
The CaWO4:Eu3+ phosphors with different doping concentrations and different sintered temperatures are synthesized using the microemulsion reaction method. After sintered at different temperatures, the samples with doping concentration of 30 or 50 mol% can obtain the brightest characteristic emissions from Eu3+ ions. At 800 ℃, moreover, the samples with doping concentrations of 0.52 mol% can emit the strongest light. It is therefore concluded that more intense emissions enable the CaWO4:Eu3+ phosphors with high doping concentrations to have great potential to be used as efficient phosphors in the future.

The content you want is available to Zendy users.

Already have an account? Click here to sign in.