Influence of Residual Stresses on the Fatigue Life of a Shot-Peened Nickel-Based Single Crystal Superalloy: From Measurements to Modeling
Author(s) -
Amélie Morançais,
Mathieu Fèvre,
Manuel François,
Nicolas Guel,
Serge Kruch,
Pascale Kanouté,
Arnaud Longuet
Publication year - 2016
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/superalloys/2016/superalloys_2016_867_876
Subject(s) - superalloy , materials science , residual stress , shot peening , shot (pellet) , peening , nickel , metallurgy , single crystal , microstructure , crystallography , chemistry