Microstructure Changes and Oxidation Resistance of Aluminized Ni-Based Single Crystal Superalloys
Author(s) -
K. Kasai,
H. Murakami
Publication year - 2016
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/superalloys/2016/superalloys_2016_719_726
Subject(s) - superalloy , microstructure , materials science , metallurgy , single crystal , crystallography , chemistry