Development of a Low-Cost Third Generation Single Crystal Superalloy DD9
Author(s) -
J. Li,
S. Liu,
Z. Shi,
X. Wang,
J. Zhao
Publication year - 2016
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/superalloys/2016/superalloys_2016_57_63
Subject(s) - superalloy , materials science , computer science , metallurgy , microstructure