Deformation Mechanisms and Microstructural Evolution of ? + ?' Duplex Aggregates Generated during Thermomechanical Processing of Nickel-Base Superalloys
Author(s) -
H. Qin,
G. Xu,
B. Zhang,
W. Zhang,
G. Zhao
Publication year - 2016
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/superalloys/2016/superalloys_2016_487_496
Subject(s) - superalloy , thermomechanical processing , materials science , duplex (building) , deformation (meteorology) , metallurgy , nickel , base (topology) , microstructure , composite material , dna , mathematical analysis , mathematics , biology , genetics