Inhomogeneous Grain Coarsening Behavior in Supersolvus Heat Treated Nickel-Based Superalloy RR1000
Author(s) -
C. Argyrakis,
D. Child,
M. Hardy,
T. Jackson,
Im Parr,
V. Saraf,
K. Severs,
J. Stumpf
Publication year - 2016
Language(s) - Uncategorized
Resource type - Conference proceedings
DOI - 10.7449/superalloys/2016/superalloys_2016_447_456
Subject(s) - superalloy , materials science , nickel , metallurgy , grain size , thermodynamics , microstructure , physics