Parameter Optimization for Electron Beam Melting of IN718 Based on Melt Pool Characterization
Author(s) -
A. Chiba,
X. Ding,
Y. Koizumi
Publication year - 2016
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/superalloys/2016/superalloys_2016_367_373
Subject(s) - characterization (materials science) , materials science , cathode ray , electron , nuclear engineering , nanotechnology , physics , nuclear physics , engineering