Development of Thermal Barrier Coating System Using EQ Coating for Advanced Single Crystal Superalloys
Author(s) -
H. Harada,
K. Kawagishi,
K. Matsumoto
Publication year - 2016
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/superalloys/2016/superalloys_2016_279_284
Subject(s) - superalloy , thermal barrier coating , materials science , coating , metallurgy , composite material , alloy