?' Phase Instabilities in High Refractory Content ?-?' Ni-Base Superalloys
Author(s) -
S. Antonov,
R. Helmink,
D. Isheim,
D. Seidman,
E. Sun,
S. Tin
Publication year - 2016
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/superalloys/2016/superalloys_2016_199_208
Subject(s) - superalloy , refractory (planetary science) , materials science , metallurgy , phase (matter) , base (topology) , alloy , chemistry , mathematical analysis , mathematics , organic chemistry