Alloys-by-Design: Towards Optimization of Compositions of Nickel-Based Superalloys
Author(s) -
D. Crudden,
A. Mottura,
R. Reed
Publication year - 2016
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/superalloys/2016/superalloys_2016_15_23
Subject(s) - superalloy , nickel , materials science , metallurgy , alloy