Oxidation Behavior of Haynes 282 in Steam at 750°C
Author(s) -
L. Tang,
B. Wang,
R. Zhou,
S. Hou,
Y. Guo
Publication year - 2014
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/2014/superalloys_2014_863_871