Comparative Performance of Three High-Strength Ni-Cr-Mo Alloys in Oilfield Simulated H2S Environment
Author(s) -
I. Van Roy,
Rashmi B. Bhavsar,
Tony Collins
Publication year - 2014
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/2014/superalloys_2014_659_665
Subject(s) - materials science , metallurgy , petroleum engineering , computer science , geology