Effect of Aging Heat-Treatment on Mechanical Properties of AD730 Superalloy
Author(s) -
Alexandre Devaux,
A. Helstroffer,
F. Pettinari-Sturmel,
J. Cormier,
J. Douin,
M. Hantcherli,
P. Villechaise
Publication year - 2014
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/2014/superalloys_2014_521_535
Subject(s) - superalloy , materials science , metallurgy , microstructure