The Golden Age of Cast Structural Superalloys
Author(s) -
R. Helmink
Publication year - 2014
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/2014/superalloys_2014_171_180
Subject(s) - superalloy , materials science , metallurgy , microstructure