Nanoindentation and Nano-compresion Testing of Ni3Al Precipitates
Author(s) -
B. Gan,
Hideyuki Murakami,
R. Maaß,
L. Meza,
J. Greer,
T. Ohmura,
S. Tin
Publication year - 2012
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/2012/superalloys_2012_83_91
Subject(s) - nanoindentation , materials science , nano , metallurgy , composite material