z-logo
open-access-imgOpen Access
Development of a New 760°C (1400°F) Capable Low Thermal Expansion Alloy
Author(s) -
M. Fahrmann,
Kartik Srivastava,
L. Pike
Publication year - 2012
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/2012/superalloys_2012_769_777
Subject(s) - alloy , thermal expansion , materials science , metallurgy