Understanding and Modeling of Grain Boundary Pinning in Inconel 718
Author(s) -
Andrea Agnoli,
Marc Bernacki,
Roland E. Logé,
J. Franchet,
J. Laigo,
Nathalie Bozzolo
Publication year - 2012
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/2012/superalloys_2012_73_82
Subject(s) - grain boundary , inconel , materials science , metallurgy , engineering physics , engineering , microstructure , alloy