Computational Fluid Dynamics Modelling of Heat Treatment of Single Crystal Nickel Based Superalloys for Turbine Blade Application
Author(s) -
F. Cosentino,
N. Warnken,
J. Gebelin,
R. Broomfield,
R. Reed
Publication year - 2012
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/2012/superalloys_2012_673_682
Subject(s) - superalloy , turbine blade , blade (archaeology) , computational fluid dynamics , materials science , turbine , nickel , gas turbines , fluid dynamics , mechanical engineering , computer science , mechanics , metallurgy , nuclear engineering , engineering , physics , microstructure
Accelerating Research
Robert Robinson Avenue,
Oxford Science Park, Oxford
OX4 4GP, United Kingdom
Address
John Eccles HouseRobert Robinson Avenue,
Oxford Science Park, Oxford
OX4 4GP, United Kingdom