Author(s) -
C. Ge,
Y. Zhang,
Y. Xu,
W. Shen,
Y. Zhang,
H. Wu
Publication year - 2012
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/2012/superalloys_2012_557_562
Subject(s) - superalloy , materials science , metallurgy , computer science , microstructure