Sustained Macroscopic Deflected Fatigue Crack Growth in Nickel Based Superalloy 720Li
Author(s) -
C. Schoettle,
P. Reed,
M.J. Starink,
Ian Sinclair,
D. J. Child,
Geoff West,
Rachel C. Thomson
Publication year - 2012
Language(s) - Uncategorized
Resource type - Conference proceedings
DOI - 10.7449/2012/superalloys_2012_395_402
Subject(s) - superalloy , materials science , nickel , paris' law , fatigue testing , metallurgy , composite material , crack closure , fracture mechanics , microstructure