Processing to Fatigue Properties: Benefits of High Gradient Casting for Single Crystal Airfoils
Author(s) -
C. Brundidge,
Tresa M. Pollock
Publication year - 2012
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/2012/superalloys_2012_379_385
Subject(s) - airfoil , casting , computer science , materials science , composite material , aerospace engineering , engineering