z-logo
open-access-imgOpen Access
Low Cycle Fatigue of CMSX-4 in Off-axis Orientations and the Effect of a Multi-axial Stress State
Author(s) -
N. Barnard,
D. MacLachlan,
N. Jones,
J. Mason-Flucke,
S. Bagnall,
M. Bache
Publication year - 2012
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/2012/superalloys_2012_293_300
Subject(s) - stereographic projection , materials science , superalloy , structural engineering , torsion (gastropod) , finite element method , isothermal process , low cycle fatigue , strain gauge , stress (linguistics) , fatigue testing , geometry , composite material , engineering , mathematics , microstructure , physics , linguistics , philosophy , medicine , surgery , thermodynamics

The content you want is available to Zendy users.

Already have an account? Click here to sign in.
Having issues? You can contact us here