Influence of γ' Precipitate Size and Distribution on LCF Behavior of a PM Disk Superalloy
Author(s) -
G. Boittin,
D. Locq,
A. Rafray,
P. Caron,
P. Kanouté,
F. Gallerneau,
G. Cailletaud
Publication year - 2012
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/2012/superalloys_2012_167_176
Subject(s) - superalloy , materials science , metallurgy , distribution (mathematics) , alloy , mathematics , mathematical analysis