Overview on 718Plus® Assessment within VITAL R&D Project
Author(s) -
O. Ruiz,
S. Sjöberg,
T. Gomez-Acebo
Publication year - 2010
Language(s) - Uncategorized
Resource type - Conference proceedings
DOI - 10.7449/2010/superalloys_2010_689_704