Characterization of Microstructures Containing Abnormal Grain Growth Zones in Alloy 718
Author(s) -
B. Flageolet,
J. Cormier,
O. Yousfi,
P. Villechaise,
Y. Dahan
Publication year - 2010
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/2010/superalloys_2010_595_606
Subject(s) - alloy , microstructure , materials science , characterization (materials science) , abnormal grain growth , metallurgy , grain growth , grain size , nanotechnology