Simulations of Temperatures, Residual Stresses, and Porosity Measurements in Spray Formed Super Alloys Tubes
Author(s) -
A.A. Becker,
Reinhold Kienzler,
Volker Uhlenwinkel,
R. Ristau
Publication year - 2010
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/2010/superalloys_2010_471_485
Subject(s) - materials science , porosity , residual stress , composite material , metallurgy , residual , porous medium , algorithm , computer science