Toughness as a Function of Thermo-Mechanical Processing and Heat Treatment in 718Plus® Superalloy
Author(s) -
S. Oppenheimer,
E. McDevitt,
W. Cao
Publication year - 2010
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/2010/superalloys_2010_321_330
Subject(s) - charpy impact test , materials science , superalloy , toughness , fractography , alloy , metallurgy , fracture toughness , grain boundary , ultimate tensile strength , microstructure , composite material