Manufacture and Property Evaluation of Super Alloy 44Ni-14Cr-1.8Nb-1.7Ti-1.5Mo-0.3V-Fe ( Modified 706 )-an Experience
Author(s) -
U. V. Gururaja,
M. Kameswara Rao,
Prasenjit Sarkar
Publication year - 2010
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/2010/superalloys_2010_237_242
Subject(s) - property (philosophy) , alloy , materials science , computer science , metallurgy , philosophy , epistemology