Influence of Portevin-Le Chatelier Effect on Rupture Mode of Alloy 718 Specimens
Author(s) -
Véronique Garat,
J-M. Cloue,
Bernard Viguier,
Éric Andrieu
Publication year - 2005
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/2005/superalloys_2005_551_557
Subject(s) - materials science , portevin–le chatelier effect , alloy , mode (computer interface) , metallurgy , dynamic strain aging , computer science , operating system