Nanoindentations as a Local Probe for the Mechanical Properties and Alloying Influences in Nickel-Base Superalloys and Aluminide Coatings
Author(s) -
Karsten Durst,
Oliver Franke,
Mathias Göken
Publication year - 2004
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/2004/superalloys_2004_467_476
Subject(s) - superalloy , materials science , aluminide , metallurgy , base (topology) , nickel , alloy , intermetallic , mathematical analysis , mathematics