Fatigue Fracture Surface Morphology for Alloy 718
Author(s) -
W. J. Mills,
C. M. Brown
Publication year - 2001
Language(s) - Uncategorized
Resource type - Conference proceedings
DOI - 10.7449/2001/superalloys_2001_511_522
Subject(s) - striation , materials science , dimple , alloy , fracture (geology) , cracking , homogeneous , slip (aerodynamics) , deformation (meteorology) , metallurgy , composite material , thermodynamics , physics