Advances in the Solidification of IN718 and RS5 Alloys
Author(s) -
Laurentiu Nastac,
Michael L. Tims,
F.R. Dax,
I Concurrent
Publication year - 2001
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/2001/superalloys_2001_103_112
Subject(s) - materials science , metallurgy