Structure/Property Interactions in a Long Range Order Strengthened Superalloy
Author(s) -
M. F. Rothman,
D. L. Klarstrom,
M. Dollár,
J.F. Radavich
Publication year - 2000
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/2000/superalloys_2000_553_562
Subject(s) - materials science , superalloy , property (philosophy) , range (aeronautics) , order (exchange) , metallurgy , composite material , business , microstructure , philosophy , epistemology , finance