Enhanced Powder Metallurgy (P/M) Processing of UDIMET Alloy 720 Turbine Disks: Modeling Studies
Author(s) -
James J. Fisher,
Albert Casagranda,
Suhas Vaze,
F. D. Arnold,
Sen Lin,
G. Salvady,
Gary A. Miller
Publication year - 2000
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/2000/superalloys_2000_143_149
Subject(s) - materials science , powder metallurgy , alloy , metallurgy , turbine , mechanical engineering , microstructure , engineering