Room Temperature Formability of Alloys 625LCF, 718 and 718SPF
Author(s) -
P. Roamer,
C. J. Van Tyne,
David K. Matlock,
Alan Meier,
H. Ruble,
Fernando Suárez Guerra
Publication year - 1997
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/1997/superalloys_1997_315_329
Subject(s) - formability , materials science , metallurgy