The Development and Application of CMSX-10
Author(s) -
G. L. Erickson
Publication year - 1996
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/1996/superalloys_1996_35_44
Subject(s) - materials science , development (topology) , systems engineering , engineering , mathematics , mathematical analysis