An Experimental Study of the Role of Plasticity in the Rafting Kinetics of a Single Crystal Ni-Base Superalloy
Author(s) -
Michael G. Fahrmann,
E Fährmann,
Oskar Paris,
Peter Fratzl,
TM Pollock
Publication year - 1996
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/1996/superalloys_1996_191_200
Subject(s) - materials science , superalloy , kinetics , crystal plasticity , base (topology) , plasticity , metallurgy , composite material , microstructure , physics , quantum mechanics , mathematical analysis , mathematics