z-logo
open-access-imgOpen Access
Investigation of Nitrogen Atomized PM Alloy 625
Author(s) -
F. J. Rizzo,
J.J. Conway,
J.F. Radavich,
Jonathan Jones
Publication year - 1994
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/1994/superalloys_1994_923_934
Subject(s) - materials science , alloy , nitrogen , metallurgy , physics , quantum mechanics

The content you want is available to Zendy users.

Already have an account? Click here to sign in.
Having issues? You can contact us here