Stress-Relaxation Behavior of Inconel 718 in Thermal and In-Pile Conditions
Author(s) -
Christophe Getrey,
D. Gilbon,
T. Magnin,
JeanMarc Cloué
Publication year - 1994
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/1994/superalloys_1994_671_671
Subject(s) - inconel , materials science , pile , stress relaxation , relaxation (psychology) , stress (linguistics) , thermal , composite material , structural engineering , thermodynamics , creep , engineering , psychology , social psychology , physics , alloy , linguistics , philosophy