Custom Age 625 Plus Alloy: A Higher Strength Alternative to Alloy 625
Author(s) -
Richard B. Frank
Publication year - 1991
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/1991/superalloys_1991_879_893
Subject(s) - alloy , materials science , metallurgy