Impact and Fracture Toughness of Investment Cast, Plasma Sprayed, and Wrought Alloy 718
Author(s) -
G.K. Bouse
Publication year - 1991
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/1991/superalloys_1991_287_296
Subject(s) - materials science , fracture toughness , alloy , plasma , metallurgy , toughness , composite material , physics , quantum mechanics