Mechanical Properties and Microstructure of Fine Grain, Centrifugally Cast Alloy 718
Author(s) -
Gerald Gapinski,
TM Devine
Publication year - 1989
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/1989/superalloys_1989_533_544
Subject(s) - materials science , microstructure , alloy , metallurgy , grain size