The Present Status of Melting Technology for Alloy 718
Author(s) -
A. Mitchell
Publication year - 1989
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/1989/superalloys_1989_1_15
Subject(s) - materials science , alloy , metallurgy