Production of Rolled Alloy 718 Billet From VADER Ingot
Author(s) -
M. A. Mccarty,
Frank Sczerzenie
Publication year - 1989
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/1989/superalloys_1989_199_206
Subject(s) - ingot , materials science , alloy , metallurgy