Creep Behavior of Magnesium Microalloyed Wrought Superalloys
Author(s) -
Peipei Ma,
Yihui Yuan,
Z.Y. Zhong
Publication year - 1988
Language(s) - Uncategorized
Resource type - Conference proceedings
DOI - 10.7449/1988/superalloys_1988_625_633
Subject(s) - materials science , creep , superalloy , grain boundary , carbide , magnesium , metallurgy , ductility (earth science) , cohesion (chemistry) , microstructure , chemistry , organic chemistry