Development of Coatings for the Protection of Gas Turbine Blades Against High Temperature Oxidation
Author(s) -
J.E. Restall
Publication year - 1984
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/1984/superalloys_1984_721_730
Subject(s) - materials science , gas turbines , turbine blade , turbine , mechanical engineering , nuclear engineering , metallurgy , composite material , engineering