Strengthening of Cobalt-Base Alloys by Secondary Precipitation of Carbides
Author(s) -
J. H. Davidson
Publication year - 1976
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/1976/superalloys_1976_275_284
Subject(s) - materials science , carbide , cobalt , precipitation , metallurgy , base (topology) , mathematical analysis , mathematics , meteorology , physics