Effects of Rare Earth Elements and Calcium Upon High Temperature Oxidation of Austenitic Heat-Resisting Alloy Containing High Silicon
Author(s) -
Tokio Fujioka,
Masayuki Kinugasa,
Shozo Iizumi
Publication year - 1976
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/1976/superalloys_1976_159_169
Subject(s) - materials science , alloy , silicon , rare earth , metallurgy , austenite , calcium , microstructure