Phase Stability of Two Investment Cast High Chromium Nickel-Base Alloys
Author(s) -
D.R. Betner,
K.E. Muszar,
E. S. Nichols
Publication year - 1968
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/1968/superalloys_1968_278_311
Subject(s) - materials science , chromium , nickel , metallurgy , phase (matter) , base (topology) , investment (military) , mathematical analysis , chemistry , mathematics , organic chemistry , politics , political science , law