The Effect of Phase Instability on the High Temperature Stress-Rupture Properties of Representative Nickel-Base Superalloys
Author(s) -
D. M. Moon,
Friedrich J. Wall
Publication year - 1968
Language(s) - English
Resource type - Conference proceedings
DOI - 10.7449/1968/superalloys_1968_115_133
Subject(s) - superalloy , materials science , stress (linguistics) , instability , nickel , phase (matter) , base (topology) , metallurgy , microstructure , mechanics , physics , mathematical analysis , linguistics , philosophy , mathematics , quantum mechanics